News & Notice
Comprehensive analysis of the quality of the resin grinding wheel
Update Time:2012-1-27      Hits:   [ Close ]
nconsistent parts or equipment leaving the furnace caused by uneven pad. More from the grinding wheel and fine-grained thin sheet products. Thin wheel when cooling too quickly shocked the bridge easily produce waste.
10 blistering. Hardening curve by product specifications to control the temperature hardening of the mixing process with strict quality control; molding temperature is too high or too low, need to adjust the temperature curing temperature, curing oven temperature control. With agent with the wrong; superhard abrasive local deformation or the entire surface of the convex surface of the expansion, and the resin was shiny, with some turtle-shaped crack. Causes: